AUSTIN, TX – Austin-based bioengineering company Reactive Surfaces announced the general availability of WMDtox™, the world’s first self-decontaminating coating that protects firearms, vehicles, equipment and uniforms by neutralizing organophosphorous chemical agents such as sarin.
WMDtox is a clear coating that has been specially formulated to meet military specs for CARC overcoats. Reactive Surfaces is providing WMDtox to Mississippi-based weapons coating company Birdsong Firearms as a weapons coating for military personnel and first responders.