Red Spot Paint and Varnish Earns Innovation Award from Chrysler
EVANSVILLE, IN – Red Spot Paint and Varnish Co. Inc. was recently presented with the 2013 Chrysler Group Supplier of the Year Award for Innovation at the annual Supplier Strategy Meeting held in Auburn Hills, MI.
The award, given by Chrysler Group LLC, was a result of collaboration between Red Spot Paint and Varnish Co. and JVIS/Seungbo to create a new technology and process that replaces chrome plating or metallic metal parts. The new technology consists of multiple, colored chrome interior trim parts using physical vapor deposition.