The Solaplex® range of bright yellow to orange inorganic pigments based on Color Index Pigment Yellow 216 has been granted a Food Contact Notification (FCN1252) by the FDA. The pigment extends the color palette and enables brilliant shades with long-lasting UV durability, good hiding power and stability at high temperatures up to 400 °C.