ADELAIDE, Australia - University of Adelaide researchers have developed a process for turning waste plastic bags into a high-tech nanomaterial.
The innovative technology uses non-biodegradable plastic grocery bags to make carbon nanotube membranes - highly sophisticated materials with a variety of potential applications including filtration, sensing, energy storage and a range of biomedical innovations.