PPG Electrocoat Primer Qualified to Aerospace Specification
SYLMAR, CA – PPG Industries’ aerospace coatings group has qualified AEROCRON™ electrocoat primer to SAE International’s Aerospace Material Specification 3144 for anodic electrodeposition primer for aircraft applications.
Qualifying Aerocron primer to the aerospace industry standard provides airframe manufacturers and subcontractors with third-party verification of its performance characteristics and attributes, according to Duane Utter, PPG Global Coatings Segment Manager, Military Coatings and Classified Products.