MIL-PRF-22750G Type III, Grade A Seafoam Green High Solids Epoxy by Sherwin-Williams meets the military specification for direct-to-metal (DTM) applications. The new product is one of the first DTM high-solids epoxies to earn approval from the Army Research Lab in Aberdeen, MD.
The two-component coating can be used in applications that specify either Grade A or Grade B finishes, including Army or Navy equipment requiring weather resistance or for interior surfaces. It offers superior corrosion resistance and satisfies the Army Research Lab’s requirements of performance to a minimum 1,000 hours of salt spray and 40 cycles of cyclic corrosion.