AkzoNobel Coatings Withstand Rigors of Motorrad Test
AMSTERDAM, The Netherlands – AkzoNobel’s coatings drew praise from German motorbike magazine Motorrad following a rigorous long-distance road test of a Honda CBR600F.
The bike was subjected to a 50,000 km test, after which it was taken apart so that any wear and tear could be assessed.