Custom Coatings Completes 30,000 Sprays of Eurac Drums and Discs
POOLE, England – Custom Coatings, part of AIC Group, has completed 30,000 wet sprays of automotive drums and discs for UK-based Eurac. Using a new semi-automated spray line and a newly developed bespoke machine, Custom Coatings is capable of spraying one part every 10 seconds. The company has been wet spraying drums and discs at a rate in excess of 500 per day since August 2013.
Working to very tight deadlines, the supply of the discs and drums has been maintained, which will end up in luxury automotive brands. They are also made for Ifor Williams Trailers where Custom Coatings helped develop and source a coating that looks good, protects against corrosion and matches the customer’s specification.