Nanoparticle-Based Coating for Aircraft Engines May Triple Service Life and Reduce Fuel Consumption
Trollhättan, Sweden - Researchers at University West in Sweden have started using nanoparticles in the heat-insulating surface layer that protects aircraft engines from heat. In tests, this increased the service life of the coating by 300 percent. Of great interest to the aircraft industry, the hope is that motors with the new layers will be in production within two years.
To increase the service life of aircraft engines, a heat-insulating surface layer is sprayed on top of the metal components. Thanks to this extra layer, the engine is shielded from heat. The temperature can also be raised, which leads to increased efficiency, reduced emissions, and decreased fuel consumption.