DeFelsko Corp. is announcing a breakthrough in coating inspection. The new PosiTector gage body accepts all coating thickness (6000), environmental (DPM), surface profile (SPG) and ultrasonic wall thickness (UTG) probes.
This innovation allows quick and easy conversion from a coating thickness gage to a surface profile gage, dew point meter or ultrasonic wall thickness gage with a simple probe change. Each probe retains its own unique calibration information allowing for full probe interchangeability. Long-form certificates of calibration are included with each probe.