Ardleigh Minerals Introduces New Bicarbonate Recycling Process
BEACHWOOD, OH – Ardleigh Minerals Inc., a recycler for the aerospace and thermal spray industries based in Beachwood, OH, has developed a process to recycle spent sodium bicarbonate blast media.
The process converts spent bicarbonate, resulting from sodium bicarbonate (or soda) blasting, into a usable product meeting pollution-control standards. It utilizes the entire spent bicarbonate and no residues remain. Items using soda blasting include wheels, deswirlers, fuel nozzles and other component parts.