WESEL, Germany – BYK Additives & Instruments has concluded an exclusive agreement with the Spanish technology research center ITENE of Valencia on the production and marketing of new clay-based additives for the packaging industry.
The technology developed by ITENE enhances the barrier properties, the mechanical resistance and the thermal stability of packaging materials based on polylactic acid (PLA).