Fly Eyes Provide Pattern for Anti-Fogging Materials
WOLLONGONG, Australia – Researchers in Australia have discovered the eye of the fly may hold the key to anti-fogging materials.
Self-cleaning windows and glasses that don’t fog up are among the innovative applications that could result from studies carried out at Australia’s University of Wollongong, where researchers turned to the common house fly for the inspiration behind a new anti-fogging material.