December 1, 2015
Made mostly from bio-preferred materials, EBECRYL® 5849 can be formulated for either UV LED-cured coatings or 100% sprayable formulations. A multifunctional polyester acrylate that provides cured films with good hardness and scratch resistance, it shows excellent thermal and mechanical properties combined with low viscosity, high cure speed and hardness. It can be cured either by EB, UV or UV LED light. Visit www.allnex.com.