Latex for Waterproofing

OMNOVA SOLUTIONS

May 2, 2016

PLIOTECĀ® WPM120 latex for waterproofing, damp-proofing and crack-prevention membranes combines superior water resistance, excellent tensile strength and good elongation properties. It features superior resistance to hydrostatic pressure and water absorption, and can be used in barrier coatings to reduce crack transmission in tile and stone floors, and as a moisture vapor barrier under all types of floor coverings. Visit www.omnova.com.