Oxea Announces Price Increases

September 18, 2016

DALLAS – Oxea announced price increases for several of its products.

The company will implement a price increase for prices in North America, Mexico and South America on 2 ethyl hexanol effective October 1, 2016, or as contracts allow. This will be in addition to the price increase effective September 2016, which was announced August 15, 2016. In North American and Mexico, 2 ethyl hexanol will increase $0.05/lb, and in South America, 2 ethyl hexanol will increase $110/mt.

Oxea will increase list and off-list prices on neopentyl glycol and trimethylolpropane effective October 1, 2016, or as contracts allow. In North American and Latin America, neopentyl glycol will increase $70/mt ($0.03/lb), and trimethylolpropane will increase $110/mt ($0.05/lb).

The company will implement a price increase for prices in North America, Mexico and South America on n-propanol, n-propyl acetate and n/i butanol, and n/i-butyl acetate, effective October 1, 2016, or as contracts allow. This will be in addition to the price increase effective September 2016, which was announced August 15, 2016. In North America and Mexico, these products will increase $0.03/lb. In South America, they will increase $66/mt.