www.pcimag.com/articles/102717-corrosion-inhibitor
EcoAir® VpCI®-337

Corrosion Inhibitor

October 31, 2016

EcoAir® VpCI®-337 is a convenient way to get the corrosion protection of VpCI-337 in an easy-to-use spray can powered by compressed air.

On its own, VpCI-337 is a powerful biodegradable waterborne vapor corrosion inhibitor used to protect metal parts and internal void spaces with a thin, environmentally friendly self-healing film. Vapor phase Corrosion Inhibitors (VpCIs) in the fluid migrate and protect metal surfaces, resulting in time and cost savings and using a minimum amount of product.

Using bag-on-valve technology, recyclable EcoAir cans are powered by compressed air and can be sprayed in any direction — even upside down — without any worries about releasing solvents, VOCs or aerosols into the atmosphere. EcoAir VpCI-337 can be safely and easily transported for use even into remote areas without the need for electricity or special spray equipment. When the can is empty, users can simply pop the top off, remove the inner bag, and throw the remaining aluminum can directly into the recycling, avoiding costly and inconvenient disposal procedures.

VpCI-337 is consistently successful in providing protection to basic metal, metalworking and packaging industries. In most cases, products protected by EcoAir VpCI-337 Fogger are ready-to-use, with no degreasing or stripping necessary. The metal will retain a clean, corrosion-free surface, and the thin protective film will not affect paintability, conductivity, appearance or any other important property of metals or alloys.

EcoAir VpCI-337 is versatile for many applications, including void-space protection, edge spring for coils, double wall spaces, complex internal cavities, deep storage of key assets, pipes and spools, and post-weld touchup.

In testing the performance capabilities of EcoAir VpCI-337, the Cortec lab found that an EcoAir can effectively sprays VpCI-337 a distance of approximately 40 inches (101.6 cm). On average, a full can will last for four and a half minutes of constant spraying. Coverage rate is approximately 0.3-1.0 fluid ounces (8.87-29.57 ml) per cubic foot (0.03 m3), meaning 4-6 ounces (118.29-177.44 ml) of spray will protect a metal void space 12.7 cubic feet (0.36 m3) in volume.

During testing, the EcoAir VpCI-337 was sprayed on carbon steel, galvanized steel, copper and aluminum panels and found to effectively protect these metals from corrosion. The biodegradable fluid is designed to protect a variety of other metals, such as hot- or cold-rolled steel, silicon steel, stainless steel, cast iron, zinc, and brass.

Visit http://www.cortecvci.com/Products/single.php?code=10049.