Polyurethane Coating
CHEMLINE 2265 is specifically formulated as an interior lining and an exterior coating for large-diameter transmission lines of potable water, waste water and raw water. The formulation adheres extremely well directly to steel and requires no primer. CHEMLINE 2265 adds long-term corrosion protection to steel substrates in even the most demanding environments. It provides an exceptional barrier against chemical corrosion of steel walls, pipes and fittings. CHEMLINE 2265 is certified to meet ANSI/NSF 61 standards for potable water by Underwriters Laboratory. It is also certified (third party) to meet or exceed all requirements of AWWA C222-08 protocol.
CHEMLINE 2265 is a fast-set, spray-applied, two-component polyurethane coating that contains 100% solids and zero VOCs. For expedited productivity and reduced labor cost, it has a cure-to-touch time of two minutes and a recoat window of two hours.
Physical properties of CHEMLINE 2265 include hardness (Shore 77 D), adhesion to steel (3850 psi), impact resistance (570 pli) and ultimate elongation (6 %).
Application of CHEMLINE 2265 is easy with a 1:1 high pressure, plural-component mix ratio. Chemline recommends Graco Reactor E-XP1 or H-XP2.
Visit www.chemline.net.