www.pcimag.com/articles/105915-additive-from-cortec
PRODUCTS.jpg

Additive from Cortec

April 1, 2019

M-120 is a water-based corrosion-inhibitor additive that does not contain heavy metals. It can be used alone or in conjunction with other inhibitors to increase the corrosion protection of both water-based and solvent-based systems, and is recommended for use in acrylic and alkyd resin systems. Visit http://cortecadditives.com/.