Conductive Coating
Creative Materials has introduced 125-19(SP)C, a flexible, non-flammable, high-temperature-resistant conductive ink and coating. This product features excellent bonding to most metal and plastic substrates and has the unique characteristic of bonding well to silicone. A key advantage of this product is that it is non-flammable, in contrast to most products that bond to silicone, therefore avoiding many conditions where use of a flammable product is prohibitive. In addition, it has a uniquely long pot life.
125-19(SP)C is a one-component system with a room-temperature shelf life of two weeks, and is screen printable and syringe dispensable. This product is also offered as a two-component product and in a carbon resistive series. Performance properties of 125-19(SP)C include volume resistivity of 0.0003 Ω-cm, heat resistance to 280 °C, and crease resistance. Typical applications include wearable electronics, high-temperature bonding, and stretchable, elastomeric conductors.