Additive from Dow

July 1, 2020

DOWSIL™ 107F additive offers improved compatibility with optimal performance at low dosage in waterborne coatings. A formulated defoamer based on silicone polyether and hydrophobic silica, it is designed for formulations serving the architectural, wood and metal coatings segments. Visit www.dow.com/coatings.