www.pcimag.com/articles/107678-single-coat-tank-lining
Corchem

Single-Coat Tank Lining

July 15, 2020

C-207 Phenol Novolac Tank Lining from CORCHEM® is an ultra-high-solids, single-coat lining offering protection against aggressive chemicals. Features include 24-hour return to service, temperature application range of 20 °F-125 °F, single-leg or plural-component spraying application, broad-spectrum chemical resistance, 98% ultra-high solids, optional low-temperature winter cure hardener, and excellent abrasive and impact resistance. Visit corchem.com.