ENCORĀ® Flex 1361 is an all-acrylic emulsion designed for waterborne acrylic cool roof and vertical wall coatings. It offers a good balance of properties and can help formulators meet ASTM D6083 Type II and CA Title 24 requirements. ENCOR Flex 1361 offers an excellent balance of tensile and elongation properties in formulations without zinc oxide. Features include weatherability, elongation, water resistance and caustic resistance.