Decovery® SP-8310 is a 37% bio-based, breathable, multi-purpose acrylic resin that enables exterior coatings with improved outdoor durability and enhanced bio-based content. Its combination of UV and water resistance with low dirt pick-up gives it excellent long-term outdoor durability. Its broad adhesion profile means it is also suitable for a wider range of substrates and application areas. It also delivers good water vapor permeability and high elongation, enabling long-lasting paint systems with high breathability and elasticity. It offers a carbon footprint reduction of up to 8% compared with non-bio-based water-based alternatives.