www.pcimag.com/articles/111404-what-does-starve-fed-really-mean
pci0623-DidYouKnow-1-1170.jpg

What Does “Starve-Fed” Really Mean?

June 5, 2023

Semibatch emulsion polymerizations are predominately run in “starve-fed” mode, but what does that really mean? It is generally understood to mean that the monomer concentration in the particles is maintained at a level well below its maximum (saturation) value, which is ~5-7 M, depending on the monomers. Typically monomer concentration in the particles is kept at ~0.5-1 M by varying the monomer feed rate, but this can vary significantly depending on the specific process. There are two main reasons for running in “starve-fed” mode, and your selection of how starved you want to run your process depends on the relative value you attach to each objective:

  1. Maintaining low monomer concentration in the particles decreases the overall polymerization rate so that the reaction temperature can be controlled.
  2. Much better control of the copolymer composition distribution can be obtained because composition drift can be largely eliminated (more starved gives better control).

However, other factors are also important and should be considered. The overall reaction rate is roughly proportional to the number of particles, so for a given heat-removal capacity in your reactor, smaller size particles (higher particle number) require lower monomer concentration in the particles. This means that a change in particle size likely requires a change in monomer feed rate.

But, it is not that straightforward. Reducing monomer concentration also decreases molecular weight. Possibly even more significant if acrylates are involved, is that lower monomer concentration may result in more branching and crosslinking, which could impact multiple properties including film formation. Temperature is also an important factor; higher reaction temperatures give a larger temperature difference between the jacket and reactor, thereby allowing reactions to be run faster (thus you can use higher monomer concentration in the particles). Finally, comonomer composition must be considered. If there are large differences in the water solubility of the monomers, a more starved system will reduce the impact of having appreciable amounts of hydrophilic monomers (e.g. functional acids, hydroxy functional monomers) in the aqueous phase and not in the particles.

 

As always, we welcome your comments and questions by contacting us via our website, www.epced.com.