Image credit: DKosig / iStock via Getty Images Plus.
Newly Designed Nanomaterial Shows Promise as Antimicrobial Agent
Newly developed halide perovskite nanocrystals (HPNCs) show potential as antimicrobial agents that are stable, effective and easy to produce. After almost three years, Rice University scientist Yifan Zhu and colleagues have developed a new HPNC that kills bacteria in a biofluid under visible light without experiencing the light- and moisture-driven degradation common in HPNCs. A new method using two layers of silicon dioxide, which Zhu and colleagues developed over years of work, was used in experiments with lead-based and bismuth-based HPNCs to test their antimicrobial efficacy and stability in water. The study is published in Nano Letters.
Yifan Zhu, postdoctoral research associate and Jun Lou, professor and associate chair of materials science and nanoengineering.HPNCs have unique optical and electrical properties that make them promising candidates for solar power applications, bioimaging and photocatalysis, the acceleration of chemical reactions caused by light in the presence of a catalyst. One such reaction is the production of reactive oxygen species that can inactivate biological contaminants in fluids. However, perovskites are highly prone to degradation in water and biological fluids, limiting their potential in biomedical applications.
"The drawback with these materials has been stability. They're cheap and easy to make but prone to degradation," said Jun Lou, professor and associate chair of materials science and nanoengineering and a co-author of the study.
The potential for HPNCs to eliminate contaminants from water has gained attention in recent years with rising concerns about emerging pathogens and increasing rates of antibiotic resistance. Research has found that HPNCs can kill bacteria in aqueous environments by producing reactive oxygen species when exposed to light. Reactive oxygen species like singlet oxygen and hydroxide react with the proteins, lipids and genetic material in bacterial cells, effectively destroying them.
Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) images of water-stable SiO₂-coated perovskite quantum dots.
Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) images of water-stable SiO₂-coated perovskite quantum dots.In their early attempts to produce a coated HPNC, the researchers used a single layer of silicon dioxide, a material that protects the perovskite while allowing light transmission. However, a single layer had limited effectiveness, with HPNCs losing 63% of their antimicrobial ability within one day. A thicker layer could hinder or even prevent HPNCs' mechanism of action.
"Transfer of energy from perovskites can produce reactive oxygen species," said Zhu, a postdoctoral research associate in Lou's lab. "The challenge is to get the right thickness to protect the perovskite while still allowing energy transfer."
Zhu and colleagues developed a method that coats the HPNCs in two layers of silicon dioxide. After multiple attempts, the research team devised a strategy to consistently achieve optimal thicknesses for both layers.
"Two coats are more effective than one thicker coat," Lou said. "It's not just an extension of thickness. We needed a strategy because the coating has to be processed in specific ways."
Next, the researchers tested the antimicrobial properties and durability of their new double-coated HPNCs. They selected lead and bismuth because HPNCs made with both metals are highly effective under visible light and produce singlet oxygen rather than hydroxide, which can harm other organisms. Zhu and colleagues found that both HPNC varieties showed little to no antimicrobial properties without light. However, under relatively low levels of visible light, both HPNCs destroyed more than 90% of E. coli bacteria in the solution after six hours. Additionally, both HPNCs showed very little degradation over the four-day test period.
The double-layer silicon dioxide coating proved effective at protecting HPNCs from degradation while allowing energy transfer. The researchers also noted an additional benefit from the coating. Analysis found that after four days in water, the lead-based HPNCs had leached only a small amount of lead into their surroundings.
"The leaching amount of lead was well below [World Health Organization] limits," Zhu said.
The lead-based HPNCs had the best antimicrobial performance, but the bismuth-based materials also performed well.
"The benefit of bismuth is avoiding the use of lead, which is always a concern if put into the body," Lou said. "You want to find the right balance with a material that has good enough performance and that is safe."
The study findings show that HPNCs coated with two layers of silicon dioxide have the potential for use as photocatalytic antimicrobial agents. Eliminating organic contaminants like bacteria in water makes these materials a good candidate for water treatment. Further research could lead to HPNCs that address other water contaminants and even be used in therapeutics. Such materials will need further testing under real-life conditions in the field and must pass safety tests. However, the findings suggest that HPNCs could be useful in various applications.
"After many years of investment in research into these materials, they are approaching reality," Lou said.
This work was supported by NSF ERC on Nanotechnology-Enabled Water Treatment (NEWT) under award EEC-1449500 and NSF I/UCRC Center for Atomically Thin Multifunctional Coatings (ATOMIC) under award EEC-2113882.