www.pcimag.com/articles/113273-fumed-silica-matting-agent-enhances-clarity-and-surface-smoothness
WoodCoatings-123946969.jpg
Image courtesy of Cabot Corporation.

Image courtesy of Cabot Corporation. 

Fumed Silica Matting Agent Enhances Clarity and Surface Smoothness

February 26, 2025

Cabot Corporation has introduced CAB-O-SIL® MT-6460, a dry fumed silica matting agent designed for wood and leather coatings. This additive delivers efficient matting performance, a smooth surface appearance, and superior clarity at lower loadings. Suitable for water-based acrylics, polyurethanes, and epoxy resins, it supports the transition to water-based systems by reducing solvent use by up to 60% compared to traditional solvent-based formulations. Additionally, CAB-O-SIL MT-6460 can achieve the same gloss level as organic wax with 50% less material, offering a cost-effective solution for formulators. The additive is also applicable in printing inks, packaging, ultraviolet, and non-polar systems.

Learn more here.