Evonik introduced TEGO® Wet 288, a substrate wetting additive designed for waterborne and radiation-curable inks and coatings. It offers stable performance in high pH waterborne formulations and supports wetting without compromising reprintability or glueability in radiation-cured systems.
In inkjet inks, the additive helps reduce surface tension and maintains effectiveness over time. It also meets broad food contact compliance requirements, enabling use in food packaging applications.