www.pcimag.com/articles/82631-thickener

Thickener

September 1, 2003
Avecia

This company has introduced SOLTHIX(tm) A100 polymeric associative thickener. Based on acrylic technology, the product is extremely efficient at delivering high viscosity at low shear - with lower dosages required to achieve excellent anti-settling and anti-sag performance. The product is directly incorporated into the paint, with a process step being saved, as no pre-gel preparation is required. SOLTHIX(tm) A100 complements SOLTHIX(tm) 250, which prevents thermal sag with minimal effect on gloss in a wide range of solvent-based paint applications. For more information, call +44 (0) 161 721 2942 or e-mail roger.johnstone@avecia.com.