www.pcimag.com/articles/82800-measure-orange-peel-and-doi

Measure Orange Peel and DOI

February 1, 2005
BYKGardener



Measure Orange Peel and DOI
BYK-Gardner
The micro-wave-scan allows the measuring of orange peel and distinctness of image (DOI) on small and curved parts, like bumpers, gas tank doors, mirror housings or motorcycle parts. The instrument measures long wave and short wave. The structure spectrum offers additional information and assists in optimizing and troubleshooting. The small, lightweight unit fits in the palm of the hand, and is operated with a scroll wheel. A large display shows complete statistics and allows the input of alphanumeric names. Call 800/343.7721.