www.pcimag.com/articles/82810-ultraviolet-systems-and-basf-develop-3-d-uv-curing-system
Ultraviolet Systems and BASF Develop 3-D UV-Curing System
February 1, 2005
HOUSTON - Ultraviolet Systems has introduced a low-cost, low-energy, environmentally friendly and efficient 3-D curing system using UV energy and the patented Larolux® process from BASF.
For more information, please e-mail Ultraviolet Systems at info@uvbiz.com or visit the website www.uvbiz.com.