Fusion UV Systems Granted Patent for Improved UV Coatings

August 1, 2005
GAITHERSBURG, Md. - Fusion UV Systems, Inc., has been granted US patent 6,908,586 B1, "Free Radical Polymerization Method Having Reduced Premature Termination, Apparatus for Performing the Method, and Product Formed Thereby." The patent supports the company's Light Hammer® line of high-intensity UV lamps for industrial UV curing. It applies to the enhanced level of curing that results when substantially constant UV is used to cure coatings and inks.

For more information, visit www.fusionuv.com.