www.pcimag.com/articles/82980-pumps
Pumps
October 1, 2003

Magnatex[R] Pumps, Inc.
Texel[R] MTA Series pumps feature an ANSI-compatible design combined with a chemically inert PFA lining. The pump conforms to ANSI B73.3M hydraulic and dimensional standards, thus preventing the need to alter piping or base plates of existing ANSI installations. Its sealless, magnetic-drive design eliminates the need for costly mechanical seals. The pump’s PFA fluoropolymer lining offers chemical corrosion resistance. Call 713/972.8666 or e-mail sales@magnatexpumps.com.