Interpolymer Corp.

Megatran® 233 is a new polymer for high-solids durable floor finishes with superior scuff and scratch resistance. When properly formulated, it produces very durable floor-finish formulations that feature excellent gloss characteristics and require very little maintenance. Due to high-solids content, formulations based on the patented Megatran 233 polymer require fewer coats than are needed with conventional lower-solids formulations. Contact 800/262.1281 or e-mail info@interpolymer.com.