Orange Pigment

December 1, 2003
Engelhard Corp.

This company has introduced a new red-shade orange pigment for use in industrial coatings that offers better weather-fastness than alternative pigments without an increase in cost. Synergy Orange 6118 showed a significant improvement over Pigment Orange 34 in accelerated weathering studies conducted in the company's laboratories, resulting in improved performance at no increase in cost for most formulations. For more information, visit www.engelhard.com.