www.pcimag.com/articles/84026-spectrodensitometer
Spectrodensitometer
June 30, 2002
X-Rite
The 939 portable 0deg/45deg spectrodensitometer is now offered. The instrument features the company's 31-point spectral engine, which yields an average agreement of .15 delta E and a maximum of .30 delta E. The instrument can store more than 3,000 color references and samples, is easy to calibrate for black/white or color validation, and comes in a rugged case. Circle No. 151