www.pcimag.com/articles/84083-doverslip-er-and-or
DoverSlip ER and OR
August 1, 2002
Dover Chemical Corp. has created DoverSlip ER and OR. The refined vegetable-based amide additives are nontoxic, noncorrosive and have extremely low acid value. The materials can improve slip and antiblock properties in wax- and resin-coated papers. Circle No. 210