www.pcimag.com/articles/84577-coating-measurement-1

Coating Measurement

March 1, 2004


DeFelsko Corp.

The PosiTector 200 is an easy-to-use, affordable gage for non-destructive measurement of coating thickness on wood, concrete and more. Familiar features include a two-button, menu-driven user interface; large, easy-to-read LCD; internal memory of 1000 readings; and flip display. The unit is ready to measure right-out-of-the-box. Call 800/448.3835.