Elcometer Instruments: Coating Thickness

March 27, 2001
A new palm-sized coating thickness gauge is available that uses the measurement techniques of electromagnetic induction and eddy currents to measure on ferrous and nonferrous substrates. The model 456 incorporates a graphics display that offers menu-driven operation.