Pretreatment System for Powder Coating by Atotech

August 1, 2004
Atotech

The UniPrep™ Pretreatment System for powder coating helps eliminate formation of scale and sludge, frequent dumping of solutions, and higher operating temperatures, thereby providing less maintenance, reduced waste treatment and increased energy savings. UniPrep™ is a clean, phosphate-free process, which can eliminate the need for frequent and costly tank and spray nozzle cleaning. The process employs bioremediation, which naturally converts soils and oils into carbon dioxide and water, thereby eliminating the need for regular process solution dumping. Call 803/817.3500.