NanoShield™ ZN-3010 and NanoShield ZN-3012 are dispersions of zinc oxide in water designed to be incorporated in coatings applied to a fabric or non-woven substrates. Zinc oxide is generally used to provide UVa and UVb blocking, as well as anti-reddening and anti-inflammatory skin effects, antimicrobial activity and odor control. These patent-pending dispersions are unique due to their high solids concentrations, typically 30-50% by weight; high stability, typically one year; and non-agglomerated nanoparticles that are typically 60 nanometers. Call 630/771.6730.