www.pcimag.com/articles/85539-correction-1
Correction
April 1, 2006
Dear Editor,
Regarding the PCI Magazine article on new technology, February 2006 issue, page 56, please note that DuPont was the first company to commercialize fluorinated additive technology, as reported by PCI in September 1999. DuPont continues to sell Zonyl® coating additives globally today, which provide easy-clean paint benefits to consumers. This technology is also used globally by some of our customers under license of our Teflon® brand.
We would appreciate a correction in your magazine.
Sincerely,
Christopher J. Martin
Market Segment Leader
DuPont Chemical
Solutions Enterprise