The Ultraliner PRO55M is a smooth-walled liner designed for UN performance tests. Made from blow-molded FDA-approved LPDE with an average wall thickness of 18-30 mils, it can protect steel drums from contaminants and keep them reusable or recyclable. The liner has an ultrathin lip that prevents leakage between the insert and drum, and provides secure drum closure. Circle No. 213
The Ultraliner PRO55M is a smooth-walled liner designed for UN performance tests. Made from blow-molded FDA-approved LPDE with an average wall thickness of 18-30 mils, it can protect steel drums from contaminants and keep them reusable or recyclable. The liner has an ultrathin lip that prevents leakage between the insert and drum, and provides secure drum closure. Circle No. 213