www.pcimag.com/articles/86071-powder-thickness-gauge-1
Powder Thickness Gauge
November 1, 2004
Elcometer, Inc.
The Elcometer 550 powder thickness gauge uses a novel, non-contact measurement technique based on a high-frequency ultrasonic transducer to predict the final cured thickness of uncured coating powders on a range of substrates. Fully portable, this easy-to-use gauge provides accurate and quick measurements. Call 800/521.0635.