www.pcimag.com/articles/86367-powdered-polyurethane-based-associative-thickener

Powdered polyurethane-based associative thickener

September 20, 2001
Borchers GmbH offers Borchi gel VP 0130, a powdered polyurethane-based associative thickener. The material can be incorporated directly into the mill base or added subsequently. It is suitable for thickening emulsion paints, and can be used to thicken other binder formulations. Circle No. 111