Reichhold: epoxy dispersion

April 6, 2000
Reichhold offers Epotuf® 37-147, a zero-VOC, waterborne epoxy dispersion designed for use in high-performance institutional coatings or in architectural applications as a crosslinker for amine of carboxyl-functional latex. The material is solvent- and odor-free, and can deliver good solvent, chemical, and humidity resistance.