Adhesion Promoters

April 20, 2007
BYK-Chemie: Company offers two innovative adhesion promoters - BYK®-4500 and BYK®-4510.

BYK-Chemie: Company offers two innovative adhesion promoters - BYK®-4500 and BYK®-4510. BYK-4500 improves the adhesion of waterborne coatings, even on rough-ground substrates due to its strong pigment affinic groups. The effect is based on a new process for which the patent is pending. BYK-4510 is an adhesion promoter for one-coat stoving systems for industrial coatings. The effect of the additive is based on a high affinity with the metal substrate and with the binder in the coating. It therefore improves the adhesion on untreated, galvanized and hot-dip galvanized steel, as well as on aluminum and other metals. Visit www.byk-chemie.com.