RAHN:
GENOMER 2235 is a low-viscosity, aliphatic epoxy diacrylate.
RAHN: GENOMER 2235 is a low-viscosity, aliphatic epoxy diacrylate. It is a resin for radically curable inks, coatings and adhesives. It is recommended for applications where high reactivity and low viscosity are required, and is used in fast-curing formulations, producing chemically resistant and strong, but still flexible, films. Visit www.rahn-group.com.
RAHN: GENOMER 2235 is a low-viscosity, aliphatic epoxy diacrylate. It is a resin for radically curable inks, coatings and adhesives. It is recommended for applications where high reactivity and low viscosity are required, and is used in fast-curing formulations, producing chemically resistant and strong, but still flexible, films. Visit www.rahn-group.com.