www.pcimag.com/articles/87701-uv-curing-system
UV-Curing System
April 1, 2008
The MULTICURE™ UV-Curing System features a hand-held quartz lamp that produces a narrow-band 365nm output (other spectrums available) for curing three-dimensional surfaces coated with UV-curable coatings or adhesives.


UV III Systems Inc.: The MULTICURE™ UV-Curing System features a hand-held quartz lamp that produces a narrow-band 365nm output (other spectrums available) for curing three-dimensional surfaces coated with UV-curable coatings or adhesives. To operate, just scan the defocused lamp 3” to 8” above the part that requires curing for 10 to 30 seconds. It is ideal for use with UV-formulated polyesters, epoxies and composites. The lamp head is made of stainless steel and aluminum, with a comfortable handle. The power supply uses 110/120V 60 Hz.
Visit www.uv3.com.