www.pcimag.com/articles/89075-pigments-offer-a-new-family-of-colorants-based-on-diffractive-effects
Pigment
July 1, 2009
Nubiola Inorganic Pigments: A zinc-free, non-toxic anticorrosive pigment, Nubirox 302 is an organophilized calcium strontium phosphosilicate. It is an organic, water- and solventborne surface-treated pigment designed to increase anticorrosive efficiency and performance in a variety of paint systems.
www.nubiola.com
www.nubiola.com